LF-8160 Combined Corrosion and Weathering: Validating a Concept With Over a Decade of Research

Technical Articles

Posted 2013

Last Updated 2013


When coatings degrade from UV exposure, they can become more susceptible to corrosion attack. In the early 1990s, ISO and ASTM standardized a combined corrosion/weathering cycle. Today, this is still considered the most effective test method for determining the usefulness of industrial maintenance coatings.