LU-8001
The QUV® accelerated weathering tester can be used to test a wide variety of specimens. Coatings, plastics, and films are easily accommodated in the QUV tester using standard flat panel specimen holders. Other specimens can be mounted using specialty holders. Q-Lab also offers custom specimen holders for unique needs. All of Q-Lab’s specimen holders are designed to meet the requirements of ASTM G154, ISO 4892-3, and other international standards.