LW-6039 - Accelerated Weathering of Vinyl Siding

Technical Articles

Posted 2015

Last Updated 2015


This paper provides an overview of extensive research conducted by the Vinyl Siding Institute (VSI) on the development of new test methods for exterior plastic building products. The purpose of the VSI study was to develop an accelerated testing pro - tocol for use in certifying materials.