Architectural Decorative Coatings

31.03.2017

Decoral America is the Florida-based subsidiary of Decoral, an Italian company that manufactures “decorative coating systems”.  Their technology is based on a sublimation process to deposit decorative finishes on a wide variety of materials, including glass, plastic, metal, and ceramics. They sell “turn-key” systems that perform the complete process and also supply the full line of consumables. Their customers are OEM’s, fabricators, designers and architects who want a cost-effective ways to provide the appearance of wood, marble, and stone. Decoral technologies are used to create finishes for both indoor and outdoor applications. Their outdoor applications include both horizontal and vertical surfaces, in all climates and levels of sun exposure. 

Decoral had an interest in having its product classified as a “High Performance Material” from the American Architectural Manufacturers Association (AAMA), in order to open up new business opportunities. To do so, they performed a number of tests, which included an aggressive outdoor weathering test. They chose Q-Lab’s Florida outdoor testing services to evaluate the performance of their coatings in the bright, hot, humid South Florida conditions.

Why Q-Lab?

Decoral has been running the Qualicoat test standard in their Q-SUN xenon arc tester, so they were familiar with the quality of Q-Lab products.  They believed that they would get the same level of quality from Q-Lab testing services.  

Testing Description and Results

Decoral commissioned a five-year outdoor study, direct inland in Q-Lab’s Homestead, FL facility.  The study used a south-facing 45° exposure to meet the requirements of AAMA 2604. They exposed 12 metal panels that they had coated with their wood-grain finish – their number-one product. Q-Lab performed color, gloss, and visual evaluations (dirt, mildew, chalk, erosion) in accordance with the test.  Zero failures were observed during the test period and very little fading, discoloration, and gloss loss were experienced. Decoral is touting these as “outstanding long-term results.”

Benefits of Testing

By meeting the requirements of AAMA 2604, Decoral’s coatings are now considered “High Performance Organic Coatings for Aluminum Extrusions or Panels” by AAMA. Decoral sent out an e-mail blast highlighting their testing work (with a link to Q-Lab’s test report) to inform their customers. Enrico Piva, President of Decoral System USA, explained that projects requiring this kind of coatings from AAMA can now utilize Decoral products, opening up significant opportunities to sell their coatings. He added that “We had a great experience with Q-Lab and we value their professionalism and technical expertise. We are currently working with them to obtain our 10 year test standard, which will further increase our business”.

Örnek Çalışmalar için geri
 

Kaynaklar

Bİze Ulaşın

  1.  

Q-Lab Telefon Numaraları

Amerika Birleşik Devletleri: +1-440-835-8700
Florida ve Arizona Test Hizmetleri: +1-305-245-5600
İngiltere/Avrupa: +44-1204-861616
Almanya: +49-681-857470
Çin: +86-21-5879-7970

 
View Full Site