颜色、光泽度和机械测试标准
ASTM D1002
Standard Test Method for Apparent Shear Strength of Single-Lap-Joint Adhesively Bonded Metal Specimens by Tension Loading (Metal-to-Metal)
This test method covers the determination of the apparent shear strengths of adhesives for bonding metals when tested on a standard single-lap-joint specimen and under specified conditions of preparation and test.
ASTM D1002
单搭接接头粘接金属样品表面剪切强度的标准测试方法,该强度通过加载拉伸负荷(金属对金属)而测得
本测试方法规定了用于粘接金属的胶粘剂表面剪切强度的测定。测试时,使用标准单搭接接头样品,并在指定条件下制备与测试。
ASTM D1654
Voluntary Specification, Performance Requirements and Test Procedures for High Performance Organic Coatings on Aluminum Extrustions and Panels
This specification describes test procedures and performance requirements for high performance organic coatings applied to aluminum extrusions and panels for architectural products.
ASTM D1654
铝合金型材和板材上的高性能有机涂料的推荐规格、性能要求和测试程序
本规范描述了高性能有机涂料的测试程序和性能要求,这类涂料适用于建筑产品(铝合金型材和板材)。
ASTM D1876
Standard Test Method for Peel Resistance of Adhesives (T-Peel Test)
This test method is primarily intended for determining the relative peel resistance of adhesive bonds between flexible adherents by means of a T-type specimen.
ASTM D1876
胶粘剂抗剥离的标准测试方法(T型剥离测试)
本测试方法的主要目的是通过一个T型样品测定柔性胶粘体之间粘接接头的相对抗剥离性。
ASTM D2244
Standard Practice for Calculation of Color Tolerances and Color Differences from Instrumentally Measured Color Coordinates
This practice covers the calculation, from instrumentally measured color coordinates based on daylight illumination, of color tolerances and small color differences between opaque specimens such as painted panels, plastic plaques, or textile swatches.
ASTM D2244
计算色差、仪器测量出的颜色差异的标准测试程序
本测试方法规定了基于日光照明的仪器测量出的颜色变化的计算,不透明样品如彩板、塑料斑块或纺织品之间的色差公差和颜色的差异的计算。
ASTM D3164/M
Standard Test Method for Strength Properties of Adhesively Bonded Plastic Lap-Shear Sandwich Joints in Shear by Tension Loading
This standard covers a test method for strength properties of adhesively bonded plastic lap-shear sandwich joints in shear by tension loading.
ASTM D3164/M
通过加载拉伸负荷测量粘接塑料搭接接头剪切强度性能的标准测试方法
本标准规定了通过加载拉伸负荷测量塑料搭接接头剪切强度性能的测试方法。
ASTM D3330
Standard Test Method for Peel Adhesion of Pressure-Sensitive Tape
Standard test method for peel adhesion of pressure-sensitive tape.
ASTM D3330
压敏带材胶粘剂剥离的标准测试方法
压敏带材胶粘剂剥离的标准测试方法。
ASTM D3528
Standard Test Method for Strength Properties of Double Lap Shear Adhesive Joints by Tension Loading
This test method covers the determination of the tensile shear strengths of adhesives for bonding metals when tested in an essentially peel-free standard specimen that develops adhesive stress distribution representative of that developed in a typical low-peel production-type structural joint.
ASTM D3528
通过加载拉伸负荷测量双搭接剪切粘结接头强度性能的标准测试方法
本测试方法规定了胶粘剂金属粘接的拉伸剪切强度的测定,该基于在无剥离标准件上进行,得到的胶粘剂应力分布代表了典型的低剥离产品类结构件上的情况。
ASTM D412
Standard Test Methods for Vulcanized Rubber and Thermoplastic Elastomers - Tension
These test methods cover procedures used to evaluate the tensile (tension) properties of vulcanized thermoset rubbers and thermoplastic elastomers.
ASTM D412
硫化橡胶和热塑性弹性体张力的标准测试方法
这些测试方法描述了用来评估硫化橡胶和热塑性弹性体拉伸(张力)性能的程序。
ASTM D4214
Standard Test Methods for Evaluating the Degree of Chalking of Exterior Paint Films
These test methods cover the evaluation of the degree of chalking on white or tinted exterior paint films.
ASTM D4214
外墙涂料膜粉化程度评估的标准测试方法
本测试方法规定了白色或浅色外墙涂料膜粉化程度的评价
ASTM D5034
Standard Test Method for Breaking Strength and Elongation of Textile Fabrics (Grab Test)
This test method covers the grab and modified grab test procedures for determining the breaking strength and elongation of most textile fabrics.
ASTM D5034
纺织面料断裂强度和伸长率(抓样法)的标准测试方法
本测试方法规定了测定绝大多数纺织面料的断裂强度和断裂伸长率的抓样法和修改的抓样法的测试程序。
ASTM D5035
Standard Test Method for Breaking Force and Elongation of Textile Fabrics (Strip Method)
This test method covers raveled strip and cut strip test procedures for determining the breaking force and elongation of most textile fabrics.
ASTM D5035
纺织面料断裂强度和伸长率(条样法)的标准测试方法
本测试方法规定了测定绝大多数纺织面料的断裂强度和伸长率的条样法的测试程序。
ASTM D523
Standard Test Method for Specular Gloss
This test method covers the measurement of the specular gloss of nonmetallic specimens for glossmeter geometries of 60, 20, and 85°.
ASTM D523
光泽的标准测试方法
本测试方法规定了光泽计在60、20、和85度时非金属样品光泽度的测量;
ASTM D624
Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
This test method describes procedures for measuring a property of conventional vulcanized rubber and thermoplastic elastomers called tear strength.
ASTM D624
常规硫化橡胶和热塑性弹性体撕裂强度的标准测试方法
本测试方法描述了测量常规硫化橡胶和热塑性弹性体(称为撕裂强度)的性能的程序。
ASTM D638
Standard Test Method for Tensile Properties of Plastics
This test method covers the determination of the tensile properties of unreinforced and reinforced plastics in the form of standard dumbbell-shaped test specimens when tested under defined conditions of pretreatment, temperature, humidity, and testing machine speed.
ASTM D638
塑料拉伸性能的标准测试方法
本测试方法规定了非增强和增强塑料拉伸性能的测定,测试样品为标准哑铃形,在限定的预处理、温度、湿度和测试机速度条件下进行测试。
ASTM D660
Standard Test Method for Evaluating Degree of Checking of Exterior Paints
Since checking is not easily recognizable, this test method is intended to provide, through definition and illustrations, a means of evaluating the degree of this film failure.
ASTM D660
外墙涂料粉化程度评估的标准测试方法
由于粉化不容易辨认,此测试方法旨在通过定义和插图提供该薄膜失效程度的评估。
ASTM D661
Standard Test Method for Evaluating Degree of Cracking of Exterior Paints
This test method covers the evaluation of the degree of cracking of exterior paints by comparison with photographic standards.
ASTM D661
外墙涂料开裂程度评估的标准测试方法
本测试方法规定了与影像标准比较评估外墙涂料开裂程度的办法。
ASTM D662
Standard Test Method for Evaluating Degree of Erosion of Exterior Paints
This test method covers the evaluation of the degree of erosion of exterior paints by comparison with photographic standards.
ASTM D662
外墙涂料腐蚀程度评估的标准测试方法
本测试方法规定了与影像标准比较评估外墙涂料腐蚀程度的办法。
ASTM D6862
Standard Test Method for 90 Degree Peel Resistance of Adhesives
This test method covers the determination of the resistance-to-peel strength of an adhesive bond between one rigid adherend and one flexible adherend when tested at an angle of approximately 90 degrees under specified conditions of preparation and testing.
ASTM D6862
胶粘剂抗90度剥离的标准测试方法
本测试方法规定了刚性粘合体和柔性粘合体之间的胶粘剂接头的抗剥落强度的测定,测试时的角度约90度,在特定的制备与测试条件下进行。
ASTM D7003
Standard Test Method for Strip Tensile Properties of Reinforced Geomembranes
This test method is used to measure the strip tensile properties of reinforced geomembranes.
ASTM D7003
增强土工薄膜条样拉伸性能的标准测试方法
本测试方法用于测量增强土工薄膜条样拉伸性能。
ASTM D7004
Standard Test Method for Grab Tensile Properties of Reinforced Geomembranes
This test method is used to measure the grab tensile properties of reinforced geomembranes.
ASTM D7004
增强土工薄膜抓样拉伸性能的标准测试方法
本测试方法用于测量增强土工薄膜抓样拉伸性能。
ASTM D7087
Standard Test Method for An Imaging Technique to Measure Rust Creepage at Scribe on Coated Test Panels Subjected to Corrosive Environments
This test method covers the measurement of rust creepage area from a scribe line on painted/coated flat test panels after exposure to corrosive environments.
ASTM D7087
用成像技术测量在腐蚀环境中涂覆测试板划痕处锈蚀蠕变的标准测试方法
本测试方法规定了暴露于腐蚀环境后,从油漆/涂层平面试板划痕处开始的锈蚀蠕变区域的测量。
ASTM D714
Standard Test Method for Evaluating Degree of Blistering of Paints
This test method employs photographic reference standards to evaluate the degree of blistering that may develop when paint systems are subjected to conditions which will cause blistering.
ASTM D714
涂料起泡程度评估的标准测试方法
本测试方法采用影像参考标准评价起泡程度,当油漆系统处于会导致起泡的条件下时起泡可能会扩展。
ASTM D751
Standard Test Methods for Coated Fabrics
These test methods cover, but are not limited to, rubber-coated fabrics; that is, tarpaulins, rainwear, and similar products
ASTM D751
涂层织物的标准测试方法
本测试方法包括但不限于橡胶涂层织物,即防水油布、雨衣及类似产品
ASTM D772
Standard Test Method for Evaluating Degree of Flaking (Scaling) of Exterior Paints
This test method covers the evaluation of the degree of flaking (scaling) of exterior paints by comparison with photographic standards.
ASTM D772
外墙涂料剥落(起皮)程度评估的标准测试方法
本测试方法规定了用影像标准比较法评估外墙涂料剥落(起皮)程度的办法。
ASTM D882
Standard Test Method for Tensile Properties of Thin Plastic Sheeting
This test method covers the determination of tensile properties of plastics in the form of thin sheeting and films (less than 1.0 mm (0.04 in.) in thickness).
ASTM D882
薄塑料板拉伸性能的标准测试方法
本测试方法规定了薄片和薄膜(小于1毫米(0.04英寸)厚度)塑料拉伸性能的测定。
ISO 527
Plastics - Determination of Tensile Properties
ISO 527
塑料-拉伸性能的测定
SAE J1523
Metal to Metal Overlap Shear Strength Test for Automotive Type Adhesives, Recommended Practice
This SAE Recommended Practice defines a procedure for determining shear strengths of adhesives.
SAE J1523
汽车用胶粘剂金属和金属间的剪切强度测试,推荐做法
本SAE标准定义了测定胶粘剂剪切强度的程序。
Looking for a specific test standard? Search entire listing of all standards.
您现已登陆账户。您可以阅读所有标(
) 或 (
) 文件。想要阅读标 (
) 文件, 请注册您的设备.
您现已登陆账户。您可以阅读所有标(
) 或 (
) 文件。想要阅读标 (
) 文件, 请注册您的设备.